Welding Electrodes, Welding Consumable, Welding Rod manufacturer / supplier in China, offering Stainless Steel Electrodes Golden Bridge Welding Rod A022, Stainless Steel Welding Electrodes Lincoln / Atlantic Welding Rod E309, Stainless Steel Welding Electrodes Lincoln / Atlantic Welding Rod E308-16 and so on.

(/ )

Supplier Homepage Product Welding rod Stainless Steel Electrodes Golden Bridge Welding Rod A022

Stainless Steel Electrodes Golden Bridge Welding Rod A022

FOB Price: US $6.9-13 / KG
Min. Order: 10 KG
Min. Order FOB Price
10 KG US $6.9-13/ KG
Get Latest Price
Production Capacity: 8000mt
Transport Package: Carton
Payment Terms: L/C, T/T, Western Union, Paypal
Basic Info
  • Model NO.: A022
  • Material: Carbon Steel
  • Length: 300-350mm
  • Electrode Coating Type: Titanium Calcium
  • Stainless Steel Welding Rod Type: Stainless Steel
  • Welding Power: DC
  • Trademark: Ruitong/Golden Bridge
  • Origin: China
  • Type: E (Carbon Steel Electrodes/ Low Alloy Steel Electrodes)
  • Diameter: 2.0-5.0mm
  • Welding Core Type: Stainless Steel
  • Slag Characteristic: Acidic
  • Function: Surfacing Electrode, Low Hydrogen Type Electrode, High Efficient Iron Powder Electrode, Gravity Electrode
  • Weight: 5kg/Box, 20kg/Carton
  • Specification: 4boxes/carton
  • HS Code: 83111000
Product Description

Introduction:
A022 is a kind of Titanium calcium type coating with ultra-low carbon Cr18Ni12Mo2 stainless steel electrode. Carbon content of deposited metal is less than or equal to 0.04%. It has excellent heat resistance, the corrosion resistance, the crack resistance and the porosity resistance. Good operation performance and high strength coating. AC/DC both can be applied.
 
Uses:
Used for welding of synthetic fiber and other equipments and the same type of stainless steel structure, In addition, it is applied to weld the steel that cannot be processed with thermal treatment, such as Chromium stainless steel, clad steel, dissimilar steel, etc.
 
Chemical Composition (%)

Chemical CompositionCMnSiSPCrNiMoCu
Guarantee Value<=0.040.50~2.50<=1.00<=0.030<=0.04017.0~20.011.0~14.02.0~3.0<=0.75
General Result0.0251.200.600.0070.02119.0511.602.450.038
 
Mechanical Properties of Deposited Metal
Test ItemRm(N/mm2)A (%)
Guarantee Value>=490>=25
General Result57046
 
 
Reference Current ((AC OR DC+)
Diameter (mm)φ2.0φ2.5φ3.2φ4.0φ5.0
Welding Current (Amps)40~8050~10070~130100~160140~200

 
Notes:
1.The electrode must be preheated at the temperature of 300°C for 1 hour. Preheat the rod whenever it is used
2.As Preferred DC power supply, electric current should not be high.